DORADO NP
Ni Cr Mo Al Be Other

76

14

6
2
1.8
x

"X" denotes a content of less than one percent.

Type IV, PFM
Color White
Melting Range 2250-2355oF (1230-1290oC)
Casting Temperature 2500oF (1370oC)
Density 7.8 g/cm3
Yield Strength c =80,000 psi
Tensile Strength c =165,000 psi
Elongation c =12-15%
Vickers Hardness c =240
Investment Phosphate Bonded
Burnout Temperature 1600oF (870oC)
Oxidation 1200-1800oF (650-980oC)
Minutes/Vacuum 0/Yes
Sandblast No
Coef. of Exp. 25-500oC 14.0 um/m-K
Coef. of Exp. 25-600oC 14.4 um/m-K
Pre-Solder NP
Post-Solder LO, R
  c = cast
Caution: This alloy contains nickel and should not be used for individuals with known nickel sensitivity. This alloy contains beryllium. The dust from grinding the alloy can be toxic and should not be inhaled. Grind and polish with adequate ventilation and use a NIOSH approved respirator. Please use alloy in accordance with the MSDS sheet supplied with the product.

Dorado Dental Supply, Inc.
1010 University Ave #466
San Diego, CA 92103
800-215-6930
fax: 619-330-2552

email: info@doradodentalsupply.com

Copyright © 2005 - Dorado Dental Supply, All rights reserved.

5